The bottom tensile longitudinal reinforcement and the top longitudinal reinforcement of the specimen were selected from HRB400 hot-rolled ribbed steel bars, with the top longitudinal reinforcement diameter of 8mm and the bottom tensile longitudina...

The provided information contains the following reinforcement properties:

  • Bottom tensile longitudinal reinforcement:

    • Material: HRB400 hot-rolled ribbed steel bar
    • Diameter: 20 mm
    • Yield strength: 413.10 MPa
    • Yield strain: 2065 με
    • Tensile strength: 568.99 MPa
  • Top longitudinal reinforcement:

    • Material: HRB400 hot-rolled ribbed steel bar
    • Diameter: 8 mm
  • Hoop reinforcement:

    • Material : HPB300 smooth round steel bars
    • Diameter :8mm
    • Yield strength :407.00 MPa
    • Tensile strength :458.38 MPa

本站部分文章来源于网络,版权归原作者所有,如有侵权请联系站长删除。
转载请注明出处:https://sdn.0voice.com/?id=927

分享:
扫描分享到社交APP
上一篇
下一篇
发表列表
游客 游客
此处应有掌声~
评论列表

还没有评论,快来说点什么吧~

联系我们

在线咨询: 点击这里给我发消息

微信号:3007537140

上班时间: 10:30-22:30

关注我们
x

注册

已经有帐号?